Corrosion Resistant Nickel Based Superalloy GH3128 Alloy For Erospace Components

Corrosion Resistant Nickel Based Superalloy GH3128 Alloy For Erospace Components

MOQ: 100KG
Price: Price is negotiated based on the required specifications and quantity
Standard Packaging: Standard export packaging, or packaging as required
Delivery Period: 5-8 working days, depending on the parameters required for negotiation
Payment Method: Payment Terms: Mainly T/T.. L/C, D/A, D/P,
Supply Capacity: 5000 tons per month
Detail Information
Place of Origin
China
Brand Name
Zhonggong Special Metallurgy
Certification
ISO Certificate
Model Number
GH3128 alloy
Name:
Nickel Based Superalloy
Density:
~8.3 G/cm³
Melting Point:
~1400°C (2550°F)
Yield Strength:
~800 MPa (116 Ksi)
Ultimate Tensile Strength:
~950 MPa (138 Ksi)
Elongation:
~12%
Hardness (Rockwell):
~HRB 95-100
Applications:
Erospace Components, High-temperature Industrial Parts
Highlight:

Corrosion Resistant Nickel Based Superalloy

,

Nickel Based Superalloy GH3128

,

GH3128 Alloy

Product Description

GH3128 Alloy Is A High-Strength Nickel-Based Superalloy With Excellent Oxidation And Corrosion Resistance

 

GH3128 Alloy

GH3128 is a high-performance nickel-based superalloy renowned for its exceptional strength, oxidation, and corrosion resistance at elevated temperatures. This alloy is specifically engineered to perform reliably in harsh environments where both mechanical and thermal stresses are significant.

 

Key Features:

  • Composition: The alloy consists primarily of nickel, with key elements including chromium, iron, and cobalt, which contribute to its robust mechanical properties and resistance to oxidation.
  • Temperature Resistance: GH3128 maintains its strength and integrity at high temperatures up to approximately 1400°C (2550°F), making it suitable for extreme operating conditions.
  • Mechanical Strength: It offers high yield and tensile strength, providing superior load-bearing capabilities and durability under stress.
  • Corrosion and Oxidation Resistance: The alloy excels in resisting oxidation and corrosion, ensuring long-term performance and reliability in aggressive environments.
  • Applications: GH3128 is commonly used in aerospace applications, including turbine engines and high-temperature industrial components, where its strength and resistance to thermal and environmental degradation are crucial.

GH3128 alloy’s combination of high strength, excellent thermal stability, and superior corrosion resistance makes it an ideal material for critical aerospace and industrial applications.


This description highlights the key attributes and applications of GH3128 alloy, providing a clear overview of its benefits and uses.

 

Here is the detailed composition table for GH3128 alloy:

 

Element Content Range
Nickel (Ni) Balance
Chromium (Cr) 20.0-22.0%
Iron (Fe) 15.0-20.0%
Molybdenum (Mo) 2.0-3.0%
Cobalt (Co) 8.0-12.0%
Titanium (Ti) 1.0-2.0%
Aluminum (Al) 1.5-2.5%
Boron (B) 0.005-0.015%

This table provides a clear breakdown of GH3128 alloy's chemical composition, highlighting its key elements.

 
 
products
PRODUCTS DETAILS
Corrosion Resistant Nickel Based Superalloy GH3128 Alloy For Erospace Components
MOQ: 100KG
Price: Price is negotiated based on the required specifications and quantity
Standard Packaging: Standard export packaging, or packaging as required
Delivery Period: 5-8 working days, depending on the parameters required for negotiation
Payment Method: Payment Terms: Mainly T/T.. L/C, D/A, D/P,
Supply Capacity: 5000 tons per month
Detail Information
Place of Origin
China
Brand Name
Zhonggong Special Metallurgy
Certification
ISO Certificate
Model Number
GH3128 alloy
Name:
Nickel Based Superalloy
Density:
~8.3 G/cm³
Melting Point:
~1400°C (2550°F)
Yield Strength:
~800 MPa (116 Ksi)
Ultimate Tensile Strength:
~950 MPa (138 Ksi)
Elongation:
~12%
Hardness (Rockwell):
~HRB 95-100
Applications:
Erospace Components, High-temperature Industrial Parts
Minimum Order Quantity:
100KG
Price:
Price is negotiated based on the required specifications and quantity
Packaging Details:
Standard export packaging, or packaging as required
Delivery Time:
5-8 working days, depending on the parameters required for negotiation
Payment Terms:
Payment Terms: Mainly T/T.. L/C, D/A, D/P,
Supply Ability:
5000 tons per month
Highlight

Corrosion Resistant Nickel Based Superalloy

,

Nickel Based Superalloy GH3128

,

GH3128 Alloy

Product Description

GH3128 Alloy Is A High-Strength Nickel-Based Superalloy With Excellent Oxidation And Corrosion Resistance

 

GH3128 Alloy

GH3128 is a high-performance nickel-based superalloy renowned for its exceptional strength, oxidation, and corrosion resistance at elevated temperatures. This alloy is specifically engineered to perform reliably in harsh environments where both mechanical and thermal stresses are significant.

 

Key Features:

  • Composition: The alloy consists primarily of nickel, with key elements including chromium, iron, and cobalt, which contribute to its robust mechanical properties and resistance to oxidation.
  • Temperature Resistance: GH3128 maintains its strength and integrity at high temperatures up to approximately 1400°C (2550°F), making it suitable for extreme operating conditions.
  • Mechanical Strength: It offers high yield and tensile strength, providing superior load-bearing capabilities and durability under stress.
  • Corrosion and Oxidation Resistance: The alloy excels in resisting oxidation and corrosion, ensuring long-term performance and reliability in aggressive environments.
  • Applications: GH3128 is commonly used in aerospace applications, including turbine engines and high-temperature industrial components, where its strength and resistance to thermal and environmental degradation are crucial.

GH3128 alloy’s combination of high strength, excellent thermal stability, and superior corrosion resistance makes it an ideal material for critical aerospace and industrial applications.


This description highlights the key attributes and applications of GH3128 alloy, providing a clear overview of its benefits and uses.

 

Here is the detailed composition table for GH3128 alloy:

 

Element Content Range
Nickel (Ni) Balance
Chromium (Cr) 20.0-22.0%
Iron (Fe) 15.0-20.0%
Molybdenum (Mo) 2.0-3.0%
Cobalt (Co) 8.0-12.0%
Titanium (Ti) 1.0-2.0%
Aluminum (Al) 1.5-2.5%
Boron (B) 0.005-0.015%

This table provides a clear breakdown of GH3128 alloy's chemical composition, highlighting its key elements.

 
 