GH3044 Alloy Ni Based Superalloy With High Strength Oxidation Resistance

GH3044 Alloy Ni Based Superalloy With High Strength Oxidation Resistance

MOQ: 100KG
Price: Price is negotiated based on the required specifications and quantity
Standard Packaging: Standard export packaging, or packaging as required
Delivery Period: 5-8 working days, depending on the parameters required for negotiation
Payment Method: Payment Terms: Mainly T/T.. L/C, D/A, D/P,
Supply Capacity: 5000 tons per month
Detail Information
Place of Origin
China
Brand Name
Zhonggong Special Metallurgy
Certification
ISO Certificate
Model Number
GH3044 alloy
Nickel (Ni):
Balance
Chromium (Cr):
20.0-22.0%
Iron (Fe):
5.0-7.0%
Cobalt (Co):
1.0-2.0%
Density:
~8.4 G/cm³
Melting Point:
~1370°C (2500°F)
Thermal Conductivity:
~10-12 W/m·K
Yield Strength:
~690 MPa (100 Ksi)
Ultimate Tensile Strength:
~880 MPa (128 Ksi)
Elongation:
~15%
Highlight:

GH3044 Ni Based Superalloy

,

Ni Based Superalloy Oxidation Resistance

Product Description

GH3044 Alloy

GH3044 is a high-performance nickel-based superalloy designed for exceptional strength and oxidation resistance in high-temperature environments. This alloy is predominantly used in the aerospace and power generation industries due to its superior mechanical properties and resistance to extreme conditions.

Key Features:

  • Composition: Primarily composed of nickel, chromium, and iron, with additional elements like molybdenum, tungsten, and titanium that enhance its properties.
  • Temperature Resistance: Capable of withstanding temperatures up to approximately 1370°C (2500°F), making it ideal for applications in high-heat environments.
  • Strength: Exhibits high yield and tensile strength, providing reliable performance under stress and load conditions.
  • Oxidation Resistance: Excellent resistance to oxidation and sulfidation, ensuring longevity and durability in harsh conditions.
  • Applications: Commonly used in gas turbines, aerospace components, and other high-temperature industrial applications where strength and reliability are critical.

GH3044 alloy's unique combination of strength, temperature resistance, and corrosion resistance makes it a preferred choice for demanding engineering applications, contributing to enhanced performance and extended service life of components.


Feel free to adjust this description based on specific needs or additional features of the alloy you want to highlight.

 

Here’s a detailed composition table for GH3044 alloy:

Element Content Range
Nickel (Ni) Balance
Chromium (Cr) 20.0-22.0%
Iron (Fe) 5.0-7.0%
Molybdenum (Mo) 4.0-5.0%
Tungsten (W) 0.5-1.5%
Cobalt (Co) 1.0-2.0%
Aluminum (Al) 0.8-1.2%
Titanium (Ti) 1.0-2.0%
Boron (B) 0.005-0.015%

This table provides a clear overview of the alloy's chemical composition, crucial for understanding its performance characteristics.

 

GH3044 Alloy Ni Based Superalloy With High Strength Oxidation Resistance 0

GH3044 Alloy Ni Based Superalloy With High Strength Oxidation Resistance 1

products
PRODUCTS DETAILS
GH3044 Alloy Ni Based Superalloy With High Strength Oxidation Resistance
MOQ: 100KG
Price: Price is negotiated based on the required specifications and quantity
Standard Packaging: Standard export packaging, or packaging as required
Delivery Period: 5-8 working days, depending on the parameters required for negotiation
Payment Method: Payment Terms: Mainly T/T.. L/C, D/A, D/P,
Supply Capacity: 5000 tons per month
Detail Information
Place of Origin
China
Brand Name
Zhonggong Special Metallurgy
Certification
ISO Certificate
Model Number
GH3044 alloy
Nickel (Ni):
Balance
Chromium (Cr):
20.0-22.0%
Iron (Fe):
5.0-7.0%
Cobalt (Co):
1.0-2.0%
Density:
~8.4 G/cm³
Melting Point:
~1370°C (2500°F)
Thermal Conductivity:
~10-12 W/m·K
Yield Strength:
~690 MPa (100 Ksi)
Ultimate Tensile Strength:
~880 MPa (128 Ksi)
Elongation:
~15%
Minimum Order Quantity:
100KG
Price:
Price is negotiated based on the required specifications and quantity
Packaging Details:
Standard export packaging, or packaging as required
Delivery Time:
5-8 working days, depending on the parameters required for negotiation
Payment Terms:
Payment Terms: Mainly T/T.. L/C, D/A, D/P,
Supply Ability:
5000 tons per month
Highlight

GH3044 Ni Based Superalloy

,

Ni Based Superalloy Oxidation Resistance

Product Description

GH3044 Alloy

GH3044 is a high-performance nickel-based superalloy designed for exceptional strength and oxidation resistance in high-temperature environments. This alloy is predominantly used in the aerospace and power generation industries due to its superior mechanical properties and resistance to extreme conditions.

Key Features:

  • Composition: Primarily composed of nickel, chromium, and iron, with additional elements like molybdenum, tungsten, and titanium that enhance its properties.
  • Temperature Resistance: Capable of withstanding temperatures up to approximately 1370°C (2500°F), making it ideal for applications in high-heat environments.
  • Strength: Exhibits high yield and tensile strength, providing reliable performance under stress and load conditions.
  • Oxidation Resistance: Excellent resistance to oxidation and sulfidation, ensuring longevity and durability in harsh conditions.
  • Applications: Commonly used in gas turbines, aerospace components, and other high-temperature industrial applications where strength and reliability are critical.

GH3044 alloy's unique combination of strength, temperature resistance, and corrosion resistance makes it a preferred choice for demanding engineering applications, contributing to enhanced performance and extended service life of components.


Feel free to adjust this description based on specific needs or additional features of the alloy you want to highlight.

 

Here’s a detailed composition table for GH3044 alloy:

Element Content Range
Nickel (Ni) Balance
Chromium (Cr) 20.0-22.0%
Iron (Fe) 5.0-7.0%
Molybdenum (Mo) 4.0-5.0%
Tungsten (W) 0.5-1.5%
Cobalt (Co) 1.0-2.0%
Aluminum (Al) 0.8-1.2%
Titanium (Ti) 1.0-2.0%
Boron (B) 0.005-0.015%

This table provides a clear overview of the alloy's chemical composition, crucial for understanding its performance characteristics.

 

GH3044 Alloy Ni Based Superalloy With High Strength Oxidation Resistance 0

GH3044 Alloy Ni Based Superalloy With High Strength Oxidation Resistance 1

Sitemap |  Privacy Policy | China Good Quality Stainless Steel Round Rod Supplier. Copyright © 2025 Jiangsu Zhonggongte Metallurgical Technology Co., Ltd. . All Rights Reserved.