Element | Composition (%) |
---|---|
Nickel (Ni) | Balance |
Chromium (Cr) | 19.0 - 21.0 |
Cobalt (Co) | 10.0 - 12.0 |
Molybdenum (Mo) | 2.0 - 4.0 |
Titanium (Ti) | 2.0 - 2.5 |
Aluminum (Al) | 1.0 - 1.5 |
Carbon (C) | ≤ 0.08 |
Silicon (Si) | ≤ 0.50 |
Manganese (Mn) | ≤ 0.50 |
Boron (B) | ≤ 0.01 |