logo
products
PRODUCTS DETAILS
Home > Products >
GH4169 Alloy High Strength Ni Based Superalloy With Excellent Thermal Stability

GH4169 Alloy High Strength Ni Based Superalloy With Excellent Thermal Stability

MOQ: 100KG
Price: Price is negotiated based on the required specifications and quantity
Standard Packaging: Standard export packaging, or packaging as required
Delivery Period: 5-8 working days, depending on the parameters required for negotiation
Payment Method: Payment Terms: Mainly T/T.. L/C, D/A, D/P,
Supply Capacity: 5000 tons per month
Detail Information
Place of Origin
China
Brand Name
Zhonggong Special Metallurgy
Certification
ISO Certificate
Model Number
GH4169 alloy
Density:
~8.3 G/cm³
Melting Point:
~1400°C (2550°F)
Thermal Conductivity:
~11-13 W/m·K
Yield Strength:
~850 MPa (123 Ksi)
Ultimate Tensile Strength:
~1000 MPa (145 Ksi)
Elongation:
~12%
Hardness (Rockwell):
~HRB 95-100
Applications:
Aerospace Components, Gas Turbines, And High-temperature Engines
Highlight:

High Strength Ni Based Superalloy

,

GH4169 Ni Based Superalloy

Product Description

GH4169 Alloy

GH4169 is a high-performance nickel-based superalloy specifically designed for excellent strength and stability at elevated temperatures. It is widely used in demanding applications requiring exceptional thermal and oxidative resistance.

Key Features:

  • Composition: Composed primarily of nickel, with significant amounts of chromium, iron, and cobalt, along with molybdenum and titanium. This composition contributes to the alloy's outstanding mechanical properties and resistance to high-temperature degradation.
  • Temperature Resistance: GH4169 maintains its structural integrity and performance at temperatures up to approximately 1400°C (2550°F), making it suitable for extreme thermal environments.
  • Mechanical Strength: The alloy offers high yield and tensile strength, providing durability and reliability in high-stress applications.
  • Oxidation and Corrosion Resistance: GH4169 exhibits excellent resistance to oxidation and high-temperature corrosion, ensuring long-term performance and minimal degradation in harsh conditions.
  • Applications: It is commonly used in aerospace components, gas turbines, and other high-temperature industrial processes where strength, stability, and resistance to environmental factors are critical.

GH4169’s combination of high strength, thermal stability, and corrosion resistance makes it an ideal choice for applications requiring reliable performance under severe conditions.


This description emphasizes the key properties and typical uses of GH4169 alloy, highlighting its suitability for high-performance applications.

 

Here’s a detailed composition table for GH4169 alloy:

Element Content Range
Nickel (Ni) Balance
Chromium (Cr) 19.0-21.0%
Iron (Fe) 16.0-18.0%
Cobalt (Co) 8.0-10.0%
Molybdenum (Mo) 2.5-3.0%
Titanium (Ti) 1.8-2.2%
Aluminum (Al) 1.0-1.5%
Boron (B) 0.005-0.015%

This table provides a clear overview of the chemical composition of GH4169 alloy, detailing the content ranges of its key elements.

 
GH4169 Alloy High Strength Ni Based Superalloy With Excellent Thermal Stability 0
products
PRODUCTS DETAILS
GH4169 Alloy High Strength Ni Based Superalloy With Excellent Thermal Stability
MOQ: 100KG
Price: Price is negotiated based on the required specifications and quantity
Standard Packaging: Standard export packaging, or packaging as required
Delivery Period: 5-8 working days, depending on the parameters required for negotiation
Payment Method: Payment Terms: Mainly T/T.. L/C, D/A, D/P,
Supply Capacity: 5000 tons per month
Detail Information
Place of Origin
China
Brand Name
Zhonggong Special Metallurgy
Certification
ISO Certificate
Model Number
GH4169 alloy
Density:
~8.3 G/cm³
Melting Point:
~1400°C (2550°F)
Thermal Conductivity:
~11-13 W/m·K
Yield Strength:
~850 MPa (123 Ksi)
Ultimate Tensile Strength:
~1000 MPa (145 Ksi)
Elongation:
~12%
Hardness (Rockwell):
~HRB 95-100
Applications:
Aerospace Components, Gas Turbines, And High-temperature Engines
Minimum Order Quantity:
100KG
Price:
Price is negotiated based on the required specifications and quantity
Packaging Details:
Standard export packaging, or packaging as required
Delivery Time:
5-8 working days, depending on the parameters required for negotiation
Payment Terms:
Payment Terms: Mainly T/T.. L/C, D/A, D/P,
Supply Ability:
5000 tons per month
Highlight

High Strength Ni Based Superalloy

,

GH4169 Ni Based Superalloy

Product Description

GH4169 Alloy

GH4169 is a high-performance nickel-based superalloy specifically designed for excellent strength and stability at elevated temperatures. It is widely used in demanding applications requiring exceptional thermal and oxidative resistance.

Key Features:

  • Composition: Composed primarily of nickel, with significant amounts of chromium, iron, and cobalt, along with molybdenum and titanium. This composition contributes to the alloy's outstanding mechanical properties and resistance to high-temperature degradation.
  • Temperature Resistance: GH4169 maintains its structural integrity and performance at temperatures up to approximately 1400°C (2550°F), making it suitable for extreme thermal environments.
  • Mechanical Strength: The alloy offers high yield and tensile strength, providing durability and reliability in high-stress applications.
  • Oxidation and Corrosion Resistance: GH4169 exhibits excellent resistance to oxidation and high-temperature corrosion, ensuring long-term performance and minimal degradation in harsh conditions.
  • Applications: It is commonly used in aerospace components, gas turbines, and other high-temperature industrial processes where strength, stability, and resistance to environmental factors are critical.

GH4169’s combination of high strength, thermal stability, and corrosion resistance makes it an ideal choice for applications requiring reliable performance under severe conditions.


This description emphasizes the key properties and typical uses of GH4169 alloy, highlighting its suitability for high-performance applications.

 

Here’s a detailed composition table for GH4169 alloy:

Element Content Range
Nickel (Ni) Balance
Chromium (Cr) 19.0-21.0%
Iron (Fe) 16.0-18.0%
Cobalt (Co) 8.0-10.0%
Molybdenum (Mo) 2.5-3.0%
Titanium (Ti) 1.8-2.2%
Aluminum (Al) 1.0-1.5%
Boron (B) 0.005-0.015%

This table provides a clear overview of the chemical composition of GH4169 alloy, detailing the content ranges of its key elements.

 