logo
products
PRODUCTS DETAILS
Home > Products >
GH132 Alloy High Strength Nickel Based Superalloy Oxidation Resistant

GH132 Alloy High Strength Nickel Based Superalloy Oxidation Resistant

MOQ: 100KG
Price: Price is negotiated based on the required specifications and quantity
Standard Packaging: Standard export packaging, or packaging as required
Delivery Period: 5-8 working days, depending on the parameters required for negotiation
Payment Method: Payment Terms: Mainly T/T.. L/C, D/A, D/P,
Supply Capacity: 5000 tons per month
Detail Information
Place of Origin
China
Brand Name
Zhonggong Special Metallurgy
Certification
ISO Certificate
Model Number
GH132 Alloy
Name:
Nickel Based Superalloy
Density:
~8.6 G/cm³ (0.310 Lb/in³)
Melting Point:
~1300-1400°C (2370-2550°F)
Tensile Strength:
~950 MPa (138 Ksi)
Yield Strength:
~750 MPa (109 Ksi)
Elongation:
~15%
Thermal Conductivity:
~12 W/m·K (8.4 BTU·in/hr·ft²·°F)
Modulus Of Elasticity:
~210 GPa (30 X 10³ Ksi)
Corrosion Resistance:
Good Oxidation And Corrosion Resistance At High Temperatures
Applications:
Aerospace Components, Gas Turbines, High-temperature Structural Parts
Highlight:

Nickel Based Superalloy Oxidation Resistant

,

High Strength Nickel Based Superalloy

Product Description

GH132 Alloy Is A High-Strength Nickel-Based Superalloy With Excellent High-Temperature Stability And Oxidation Resistanc

 

GH132 Alloy is a high-performance nickel-based superalloy designed for demanding high-temperature applications. It is known for its exceptional strength and stability under elevated temperatures, making it ideal for use in aerospace and industrial environments.

Key Properties and Features:

  • High-Temperature Strength: GH132 Alloy maintains robust mechanical properties, including high tensile strength (~950 MPa or 138 ksi) and yield strength (~750 MPa or 109 ksi), at temperatures up to approximately 1300-1400°C (2370-2550°F). This makes it suitable for critical components exposed to extreme heat.
  • Oxidation and Corrosion Resistance: The alloy offers excellent resistance to oxidation and high-temperature corrosion, ensuring durability and longevity in harsh environments. This property is crucial for applications in gas turbines and other high-temperature processes.
  • Mechanical Properties: GH132 provides good elongation (~15%), which contributes to its reliability in structural applications where flexibility and toughness are essential.
  • Thermal Conductivity: With a thermal conductivity of around 12 W/m·K (8.4 BTU·in/hr·ft²·°F), the alloy effectively manages heat, reducing the risk of overheating in high-performance systems.
  • Applications: Commonly used in aerospace components, high-temperature gas turbines, and other industrial applications where high strength and resistance to thermal and oxidative degradation are critical.

GH132 Alloy’s superior performance in extreme conditions ensures it is a trusted choice for advanced engineering applications requiring high durability and reliability.

 

Here is a composition table for GH132 Alloy:

Element Composition Range (%)
Nickel (Ni) 60.0 - 65.0
Chromium (Cr) 14.0 - 16.0
Cobalt (Co) 8.0 - 10.0
Molybdenum (Mo) 2.5 - 4.0
Iron (Fe) ≤ 6.0
Titanium (Ti) 1.0 - 2.0
Aluminum (Al) 1.0 - 2.0
Carbon (C) ≤ 0.10
Manganese (Mn) ≤ 0.5
Silicon (Si) ≤ 0.5
Sulfur (S) ≤ 0.01

 

These values are general guidelines. For specific applications or precise compositions, consult with industry standards or suppliers.

 

GH132 Alloy High Strength Nickel Based Superalloy Oxidation Resistant 0

products
PRODUCTS DETAILS
GH132 Alloy High Strength Nickel Based Superalloy Oxidation Resistant
MOQ: 100KG
Price: Price is negotiated based on the required specifications and quantity
Standard Packaging: Standard export packaging, or packaging as required
Delivery Period: 5-8 working days, depending on the parameters required for negotiation
Payment Method: Payment Terms: Mainly T/T.. L/C, D/A, D/P,
Supply Capacity: 5000 tons per month
Detail Information
Place of Origin
China
Brand Name
Zhonggong Special Metallurgy
Certification
ISO Certificate
Model Number
GH132 Alloy
Name:
Nickel Based Superalloy
Density:
~8.6 G/cm³ (0.310 Lb/in³)
Melting Point:
~1300-1400°C (2370-2550°F)
Tensile Strength:
~950 MPa (138 Ksi)
Yield Strength:
~750 MPa (109 Ksi)
Elongation:
~15%
Thermal Conductivity:
~12 W/m·K (8.4 BTU·in/hr·ft²·°F)
Modulus Of Elasticity:
~210 GPa (30 X 10³ Ksi)
Corrosion Resistance:
Good Oxidation And Corrosion Resistance At High Temperatures
Applications:
Aerospace Components, Gas Turbines, High-temperature Structural Parts
Minimum Order Quantity:
100KG
Price:
Price is negotiated based on the required specifications and quantity
Packaging Details:
Standard export packaging, or packaging as required
Delivery Time:
5-8 working days, depending on the parameters required for negotiation
Payment Terms:
Payment Terms: Mainly T/T.. L/C, D/A, D/P,
Supply Ability:
5000 tons per month
Highlight

Nickel Based Superalloy Oxidation Resistant

,

High Strength Nickel Based Superalloy

Product Description

GH132 Alloy Is A High-Strength Nickel-Based Superalloy With Excellent High-Temperature Stability And Oxidation Resistanc

 

GH132 Alloy is a high-performance nickel-based superalloy designed for demanding high-temperature applications. It is known for its exceptional strength and stability under elevated temperatures, making it ideal for use in aerospace and industrial environments.

Key Properties and Features:

  • High-Temperature Strength: GH132 Alloy maintains robust mechanical properties, including high tensile strength (~950 MPa or 138 ksi) and yield strength (~750 MPa or 109 ksi), at temperatures up to approximately 1300-1400°C (2370-2550°F). This makes it suitable for critical components exposed to extreme heat.
  • Oxidation and Corrosion Resistance: The alloy offers excellent resistance to oxidation and high-temperature corrosion, ensuring durability and longevity in harsh environments. This property is crucial for applications in gas turbines and other high-temperature processes.
  • Mechanical Properties: GH132 provides good elongation (~15%), which contributes to its reliability in structural applications where flexibility and toughness are essential.
  • Thermal Conductivity: With a thermal conductivity of around 12 W/m·K (8.4 BTU·in/hr·ft²·°F), the alloy effectively manages heat, reducing the risk of overheating in high-performance systems.
  • Applications: Commonly used in aerospace components, high-temperature gas turbines, and other industrial applications where high strength and resistance to thermal and oxidative degradation are critical.

GH132 Alloy’s superior performance in extreme conditions ensures it is a trusted choice for advanced engineering applications requiring high durability and reliability.

 

Here is a composition table for GH132 Alloy:

Element Composition Range (%)
Nickel (Ni) 60.0 - 65.0
Chromium (Cr) 14.0 - 16.0
Cobalt (Co) 8.0 - 10.0
Molybdenum (Mo) 2.5 - 4.0
Iron (Fe) ≤ 6.0
Titanium (Ti) 1.0 - 2.0
Aluminum (Al) 1.0 - 2.0
Carbon (C) ≤ 0.10
Manganese (Mn) ≤ 0.5
Silicon (Si) ≤ 0.5
Sulfur (S) ≤ 0.01

 

These values are general guidelines. For specific applications or precise compositions, consult with industry standards or suppliers.

 

GH132 Alloy High Strength Nickel Based Superalloy Oxidation Resistant 0

Sitemap |  Privacy Policy | China Good Quality Stainless Steel Round Rod Supplier. Copyright © 2025 Jiangsu Zhonggongte Metallurgical Technology Co., Ltd. . All Rights Reserved.