logo
products
PRODUCTS DETAILS
Home > Products >
High Strength Nickel Based Superalloy GH4145 Alloy With Excellent Thermal Stability

High Strength Nickel Based Superalloy GH4145 Alloy With Excellent Thermal Stability

MOQ: 100KG
Price: Price is negotiated based on the required specifications and quantity
Standard Packaging: Standard export packaging, or packaging as required
Delivery Period: 5-8 working days, depending on the parameters required for negotiation
Payment Method: Payment Terms: Mainly T/T.. L/C, D/A, D/P,
Supply Capacity: 5000 tons per month
Detail Information
Place of Origin
China
Brand Name
Zhonggong Special Metallurgy
Certification
ISO Certificate
Model Number
GH4145 alloy
Density:
~8.3 G/cm³
Melting Point:
~1390°C (2530°F)
Thermal Conductivity:
~11-12 W/m·K
Yield Strength:
~700 MPa (102 Ksi)
~700 MPa (102 Ksi):
900 MPa (130 Ksi)
Elongation:
~10%
Hardness (Rockwell):
~HRB 90-95
Applications:
Aerospace Components, Gas Turbines, And High-temperature Industrial Parts
Highlight:

Nickel Based Superalloy GH4145

,

Ni Based Superalloy GH4145

Product Description

GH4145 Alloy

GH4145 is a high-performance nickel-based superalloy renowned for its exceptional strength, thermal stability, and resistance to oxidation and corrosion. It is designed for use in demanding high-temperature environments where reliability and durability are critical.

Key Features:

  • Composition: The alloy primarily consists of nickel, with substantial amounts of chromium, iron, and cobalt, alongside molybdenum, titanium, and aluminum. This composition provides a balance of mechanical strength, thermal stability, and corrosion resistance.
  • Temperature Resistance: GH4145 performs effectively at high temperatures up to approximately 1390°C (2530°F), maintaining its mechanical properties and structural integrity under extreme thermal conditions.
  • Mechanical Strength: It offers high yield and tensile strength, ensuring durability and performance under significant stress and load conditions.
  • Oxidation and Corrosion Resistance: The alloy is highly resistant to oxidation and high-temperature corrosion, which prolongs the life of components and minimizes maintenance needs.
  • Applications: GH4145 is commonly used in aerospace applications, including gas turbines, as well as in high-temperature industrial processes where its strength, stability, and resistance to harsh environments are essential.

GH4145 alloy’s superior combination of strength, thermal resistance, and corrosion protection makes it an ideal material for critical applications that require reliable performance in challenging conditions.

 

Here’s a detailed composition table for GH4145 alloy:

Element Content Range
Nickel (Ni) Balance
Chromium (Cr) 18.0-21.0%
Iron (Fe) 14.0-17.0%
Cobalt (Co) 8.0-10.0%
Molybdenum (Mo) 2.0-3.0%
Titanium (Ti) 1.5-2.5%
Aluminum (Al) 1.0-1.5%
Boron (B) 0.005-0.015%

This table provides a clear overview of the chemical composition of GH4145 alloy, detailing the content ranges of its key elements.

 

High Strength Nickel Based Superalloy GH4145 Alloy With Excellent Thermal Stability 0

products
PRODUCTS DETAILS
High Strength Nickel Based Superalloy GH4145 Alloy With Excellent Thermal Stability
MOQ: 100KG
Price: Price is negotiated based on the required specifications and quantity
Standard Packaging: Standard export packaging, or packaging as required
Delivery Period: 5-8 working days, depending on the parameters required for negotiation
Payment Method: Payment Terms: Mainly T/T.. L/C, D/A, D/P,
Supply Capacity: 5000 tons per month
Detail Information
Place of Origin
China
Brand Name
Zhonggong Special Metallurgy
Certification
ISO Certificate
Model Number
GH4145 alloy
Density:
~8.3 G/cm³
Melting Point:
~1390°C (2530°F)
Thermal Conductivity:
~11-12 W/m·K
Yield Strength:
~700 MPa (102 Ksi)
~700 MPa (102 Ksi):
900 MPa (130 Ksi)
Elongation:
~10%
Hardness (Rockwell):
~HRB 90-95
Applications:
Aerospace Components, Gas Turbines, And High-temperature Industrial Parts
Minimum Order Quantity:
100KG
Price:
Price is negotiated based on the required specifications and quantity
Packaging Details:
Standard export packaging, or packaging as required
Delivery Time:
5-8 working days, depending on the parameters required for negotiation
Payment Terms:
Payment Terms: Mainly T/T.. L/C, D/A, D/P,
Supply Ability:
5000 tons per month
Highlight

Nickel Based Superalloy GH4145

,

Ni Based Superalloy GH4145

Product Description

GH4145 Alloy

GH4145 is a high-performance nickel-based superalloy renowned for its exceptional strength, thermal stability, and resistance to oxidation and corrosion. It is designed for use in demanding high-temperature environments where reliability and durability are critical.

Key Features:

  • Composition: The alloy primarily consists of nickel, with substantial amounts of chromium, iron, and cobalt, alongside molybdenum, titanium, and aluminum. This composition provides a balance of mechanical strength, thermal stability, and corrosion resistance.
  • Temperature Resistance: GH4145 performs effectively at high temperatures up to approximately 1390°C (2530°F), maintaining its mechanical properties and structural integrity under extreme thermal conditions.
  • Mechanical Strength: It offers high yield and tensile strength, ensuring durability and performance under significant stress and load conditions.
  • Oxidation and Corrosion Resistance: The alloy is highly resistant to oxidation and high-temperature corrosion, which prolongs the life of components and minimizes maintenance needs.
  • Applications: GH4145 is commonly used in aerospace applications, including gas turbines, as well as in high-temperature industrial processes where its strength, stability, and resistance to harsh environments are essential.

GH4145 alloy’s superior combination of strength, thermal resistance, and corrosion protection makes it an ideal material for critical applications that require reliable performance in challenging conditions.

 

Here’s a detailed composition table for GH4145 alloy:

Element Content Range
Nickel (Ni) Balance
Chromium (Cr) 18.0-21.0%
Iron (Fe) 14.0-17.0%
Cobalt (Co) 8.0-10.0%
Molybdenum (Mo) 2.0-3.0%
Titanium (Ti) 1.5-2.5%
Aluminum (Al) 1.0-1.5%
Boron (B) 0.005-0.015%

This table provides a clear overview of the chemical composition of GH4145 alloy, detailing the content ranges of its key elements.

 