GH738 Alloy is a high-performance, nickel-based superalloy engineered for exceptional mechanical strength and superior oxidation resistance at elevated temperatures. It is commonly used in aerospace and industrial gas turbine applications due to its ability to maintain structural integrity under extreme conditions.
Key Features:
GH738 Alloy’s robust performance characteristics make it a preferred choice for demanding applications where reliability and durability are paramount.
Here’s a table detailing the typical chemical composition of GH738 Alloy:
Element | Content (%) |
---|---|
Nickel (Ni) | 50.0 - 60.0 |
Chromium (Cr) | 20.0 - 25.0 |
Cobalt (Co) | 7.0 - 10.0 |
Molybdenum (Mo) | 3.0 - 5.0 |
Titanium (Ti) | 2.5 - 4.0 |
Aluminum (Al) | 1.5 - 2.5 |
Iron (Fe) | Balance |
Carbon (C) | ≤ 0.08 |
Boron (B) | ≤ 0.01 |
Other Elements | Traces |
This composition provides GH738 Alloy with its high-temperature strength and resistance to oxidation and corrosion.
![]() |
MOQ: | 100KG |
Price: | Price is negotiated based on the required specifications and quantity |
Standard Packaging: | Standard export packaging, or packaging as required |
Delivery Period: | 5-8 working days, depending on the parameters required for negotiation |
Payment Method: | Payment Terms: Mainly T/T.. L/C, D/A, D/P, |
Supply Capacity: | 5000 tons per month |
GH738 Alloy is a high-performance, nickel-based superalloy engineered for exceptional mechanical strength and superior oxidation resistance at elevated temperatures. It is commonly used in aerospace and industrial gas turbine applications due to its ability to maintain structural integrity under extreme conditions.
Key Features:
GH738 Alloy’s robust performance characteristics make it a preferred choice for demanding applications where reliability and durability are paramount.
Here’s a table detailing the typical chemical composition of GH738 Alloy:
Element | Content (%) |
---|---|
Nickel (Ni) | 50.0 - 60.0 |
Chromium (Cr) | 20.0 - 25.0 |
Cobalt (Co) | 7.0 - 10.0 |
Molybdenum (Mo) | 3.0 - 5.0 |
Titanium (Ti) | 2.5 - 4.0 |
Aluminum (Al) | 1.5 - 2.5 |
Iron (Fe) | Balance |
Carbon (C) | ≤ 0.08 |
Boron (B) | ≤ 0.01 |
Other Elements | Traces |
This composition provides GH738 Alloy with its high-temperature strength and resistance to oxidation and corrosion.