MOQ: | 100KG |
Price: | Price is negotiated based on the required specifications and quantity |
Standard Packaging: | Standard export packaging, or packaging as required |
Delivery Period: | 5-8 working days, depending on the parameters required for negotiation |
Payment Method: | Payment Terms: Mainly T/T.. L/C, D/A, D/P, |
Supply Capacity: | 5000 tons per month |
Attribute | Value |
---|---|
Composition | Nickel-based superalloy containing Chromium, Cobalt, Iron, and other elements |
Density | 8.23 g/cm³ |
Melting Point | 1320-1370°C (2408-2498°F) |
Tensile Strength | 850-1100 MPa (at room temperature) |
Yield Strength (0.2% offset) | 450-700 MPa |
Elongation | 30-50% |
Thermal Conductivity | 9.8 W/m·K (at 100°C) |
Coefficient of Thermal Expansion | 13.6 µm/m·K (20-100°C) |
Electrical Resistivity | 1.10 µΩ·m (at 20°C) |
Magnetic Properties | Non-magnetic |
Element | Composition (%) |
---|---|
Nickel (Ni) | 51.0 - 55.0 |
Chromium (Cr) | 19.0 - 22.0 |
Cobalt (Co) | 15.0 - 20.0 |
Iron (Fe) | 5.0 - 9.0 |
Molybdenum (Mo) | 2.5 - 3.5 |
Titanium (Ti) | ≤ 0.70 |
Aluminum (Al) | ≤ 0.60 |
Carbon (C) | ≤ 0.08 |
Manganese (Mn) | ≤ 0.50 |
Silicon (Si) | ≤ 0.50 |
Phosphorus (P) | ≤ 0.015 |
Sulfur (S) | ≤ 0.010 |
Boron (B) | ≤ 0.006 |