NS323 Alloy nickel based superalloy High Strength Superior Corrosion Resistance

NS323 Alloy nickel based superalloy High Strength Superior Corrosion Resistance

MOQ: 100KG
Price: Price is negotiated based on the required specifications and quantity
Standard Packaging: Standard export packaging, or packaging as required
Delivery Period: 5-8 working days, depending on the parameters required for negotiation
Payment Method: Payment Terms: Mainly T/T.. L/C, D/A, D/P,
Supply Capacity: 5000 tons per month
Detail Information
Place of Origin
China
Brand Name
NS323 Alloy
Certification
ISO Certificate
Model Number
NS323 Alloy
Density:
8.2 G/cm³
Tensile Strength:
900 - 1250 MPa
Yield Strength:
450 - 750 MPa
Elongation:
18 - 28%
Thermal Conductivity:
1370 - 1420°C
Hardness:
190 - 250 HB
Corrosion Resistance:
High Resistance In Aggressive Environments
Specific Heat Capacity:
14 - 17 W/m·K
Oxidation Resistance:
Excellent At High Temperatures
Highlight:

NS323 nickel based superalloy

,

nickel based superalloy high strength

Product Description
NS323 Alloy Nickel-Based Superalloy - High Strength & Superior Corrosion Resistance
Key Attributes
Attribute Value
Density 8.2 g/cm³
Tensile Strength 900 - 1250 MPa
Yield Strength 450 - 750 MPa
Elongation 18 - 28%
Thermal Conductivity 1370 - 1420°C
Hardness 190 - 250 HB
Corrosion Resistance High resistance in aggressive environments
Specific Heat Capacity 14 - 17 W/m·K
Oxidation Resistance Excellent at high temperatures
Product Overview

NS323 Alloy is a high-performance nickel-based superalloy engineered for demanding applications requiring exceptional strength, superior corrosion resistance, and excellent thermal stability. This alloy excels in high-temperature environments where material integrity and reliability are critical.

Composition

NS323 Alloy primarily consists of:

  • Nickel (Ni): 50 - 60%
  • Chromium (Cr): 20 - 25%
  • Molybdenum (Mo): 10 - 12%
  • Iron (Fe): ≤ 10%
  • Cobalt (Co): ≤ 5%
  • Titanium (Ti): 1 - 2%
  • Carbon (C): ≤ 0.08%
  • Manganese (Mn): ≤ 1%
  • Silicon (Si): ≤ 0.5%
High-Temperature Performance

Engineered for reliable operation between 1300°C to 1500°C, NS323 Alloy maintains exceptional strength and structural integrity under thermal stress. Its high melting point makes it ideal for gas turbines, jet engines, and other extreme temperature applications.

Corrosion & Oxidation Resistance

The alloy's high chromium and molybdenum content provides outstanding resistance to oxidation and corrosion in aggressive environments. This makes it particularly effective for chemical processing and power generation applications.

Mechanical Properties

NS323 Alloy combines high tensile strength (900-1250 MPa) and yield strength (450-750 MPa) with good elongation (18-28%). Its hardness (190-250 HB) and fatigue resistance ensure reliability in high-stress applications.

Fabrication & Weldability

NS323 Alloy offers excellent weldability and machinability, allowing fabrication into complex components using standard welding techniques. Proper welding practices are essential to maintain the alloy's properties.

Applications

This alloy serves critical roles in demanding industries:

  • Aerospace: Turbine blades, engine components, high-temperature fasteners
  • Power Generation: Gas turbines, steam turbines, heat exchangers
  • Chemical Processing: Equipment exposed to high temperatures and corrosive environments
  • Marine & Petrochemical: High-stress components in harsh conditions
Summary

NS323 Alloy is a versatile, high-performance material engineered for extreme temperature and corrosive environments. Its combination of strength, oxidation resistance, and fabrication characteristics makes it ideal for industrial applications requiring durability and reliability.