Name | Inconel 617 |
Chemical Composition | Ni (50.0-55.0%), Cr (20.0-24.0%), Co (12.0-15.0%), Mo (8.0-10.0%), Al (0.9-1.3%), Ti (0.4-0.6%), C (0.08% max), Mn (0.5% max), Si (0.5% max), S (0.015% max), P (0.015% max) |
Tensile Strength | 690 MPa (100 ksi) |
Yield Strength | 310 MPa (45 ksi) |
Elongation | 30% (minimum) |
Modulus of Elasticity | 210 GPa |
Density | 8.2 g/cm³ |
Melting Point | 1370-1420°C |
Thermal Conductivity | 11.0 W/m·K |
Specific Heat Capacity | 0.43 J/g·K |
Corrosion Resistance | Excellent resistance to oxidation, carburization, and high-temperature environments |
Inconel 617 is a high-performance nickel-chromium-cobalt alloy designed to provide exceptional strength and resistance to oxidation and carburization at elevated temperatures. Engineered for demanding applications, Inconel 617 is used in environments where high temperature, corrosion, and mechanical stresses are significant.
Inconel 617 is designed for optimal performance in harsh environments, offering a combination of high strength, excellent oxidation resistance, and thermal stability for critical applications in extreme conditions.
Element | Range | Typical Value |
---|---|---|
Nickel (Ni) | 50.0 - 55.0% | 52.0% |
Chromium (Cr) | 20.0 - 24.0% | 22.0% |
Cobalt (Co) | 12.0 - 15.0% | 13.5% |
Molybdenum (Mo) | 8.0 - 10.0% | 9.0% |
Aluminum (Al) | 0.9 - 1.3% | 1.1% |
Titanium (Ti) | 0.4 - 0.6% | 0.5% |
Carbon (C) | ≤0.08% | 0.05% |
Manganese (Mn) | ≤1.0% | 0.8% |
Silicon (Si) | ≤0.5% | 0.4% |
Sulfur (S) | ≤0.015% | 0.01% |
Phosphorus (P) | ≤0.015% | 0.01% |