Density | 8.14 g/cm³ |
Melting Range | 1280-1345°C |
Tensile Strength | Up to 1380 MPa (200 ksi) at room temperature |
Yield Strength | 1000 MPa (145 ksi) at room temperature |
Elongation | 20-30% |
Hardness (HB) | 277-302 HB |
Thermal Conductivity | 10.3 W/m·K at 100°C |
Coefficient of Thermal Expansion | 13.6 µm/m·K (20-100°C) |
Electrical Resistivity | 1.12 µΩ·m at 20°C |
Modulus of Elasticity | 196 GPa (28.4 x 10^6 psi) |
Magnetic Properties | Non-magnetic |
Element | Percentage Range |
---|---|
Nickel (Ni) | 42-46% |
Iron (Fe) | 33-38% |
Chromium (Cr) | 11-14% |
Titanium (Ti) | 2.6-3.4% |
Aluminum (Al) | 0.35-0.75% |
Manganese (Mn) | 0.0-0.35% |
Silicon (Si) | 0.0-0.4% |
Sulfur (S) | 0.0-0.02% |
Copper (Cu) | 0.0-0.2% |
Carbon (C) | 0.0-0.1% |
Cobalt (Co) | 0.0-0.1% |
Phosphorus (P) | 0.0-0.015% |