Attribute | Value |
---|---|
Density | ~8.8 g/cm³ (0.317 lb/in³) |
Melting Point | ~1350-1450°C (2460-2640°F) |
Tensile Strength | ~950 MPa (138 ksi) |
Yield Strength | ~800 MPa (116 ksi) |
Elongation | ~15% |
Thermal Conductivity | ~12 W/m·K (8.4 BTU·in/hr·ft²·°F) |
Modulus of Elasticity | ~210 GPa (30 x 10³ ksi) |
Corrosion Resistance | Excellent oxidation and corrosion resistance at high temperatures |
Applications | Aerospace components, gas turbines, high-temperature structural parts |
Element | Composition Range (%) |
---|---|
Nickel (Ni) | 60.0 - 65.0 |
Chromium (Cr) | 15.0 - 20.0 |
Cobalt (Co) | 5.0 - 10.0 |
Molybdenum (Mo) | 3.0 - 5.0 |
Iron (Fe) | ≤ 6.0 |
Titanium (Ti) | 1.0 - 2.0 |
Aluminum (Al) | 1.0 - 2.0 |
Carbon (C) | ≤ 0.10 |
Manganese (Mn) | ≤ 0.5 |
Silicon (Si) | ≤ 0.5 |
Sulfur (S) | ≤ 0.01 |