MOQ: | 100KG |
Price: | Price is negotiated based on the required specifications and quantity |
Standard Packaging: | Standard export packaging, or packaging as required |
Delivery Period: | 5-8 working days, depending on the parameters required for negotiation |
Payment Method: | Payment Terms: Mainly T/T.. L/C, D/A, D/P, |
Supply Capacity: | 5000 tons per month |
Attribute | Value |
---|---|
Density | ~8.3 g/cm³ |
Melting Point | ~1390°C (2530°F) |
Thermal Conductivity | ~11-13 W/m·K |
Yield Strength | ~700 MPa (102 ksi) |
Ultimate Tensile Strength | ~900 MPa (130 ksi) |
Elongation | ~10% |
Hardness (Rockwell) | ~HRB 90-95 |
Applications | Aerospace components, gas turbines, and high-temperature engines |
Element | Content Range |
---|---|
Nickel (Ni) | Balance |
Chromium (Cr) | 19.0-21.0% |
Iron (Fe) | 9.0-11.0% |
Cobalt (Co) | 8.0-10.0% |
Molybdenum (Mo) | 2.0-3.0% |
Titanium (Ti) | 2.0-3.0% |
Aluminum (Al) | 1.0-2.0% |
Boron (B) | 0.005-0.015% |