Attribute | Value |
---|---|
Density | ~8.8 g/cm³ (0.317 lb/in³) |
Melting Point | ~1300-1400°C (2370-2550°F) |
Tensile Strength | ~900 MPa (130 ksi) |
Yield Strength | ~700 MPa (102 ksi) |
Elongation | ~15% |
Thermal Conductivity | ~13 W/m·K (9 BTU·in/hr·ft²·°F) |
Modulus of Elasticity | ~210 GPa (30 x 10³ ksi) |
Corrosion Resistance | Good oxidation and corrosion resistance at high temperatures |
GH136 Alloy is a high-performance nickel-based superalloy engineered for superior strength and oxidation resistance at elevated temperatures. This alloy is designed to perform reliably in extreme environments, making it suitable for demanding applications in aerospace and high-temperature industrial processes.
GH136 Alloy's combination of high strength, oxidation resistance, and thermal stability ensures it is a reliable choice for advanced engineering applications demanding exceptional performance under extreme conditions.
Element | Composition Range (%) |
---|---|
Nickel (Ni) | 60.0 - 65.0 |
Chromium (Cr) | 14.0 - 16.0 |
Cobalt (Co) | 8.0 - 10.0 |
Molybdenum (Mo) | 3.0 - 5.0 |
Iron (Fe) | ≤ 6.0 |
Titanium (Ti) | 1.0 - 2.0 |
Aluminum (Al) | 1.0 - 2.0 |
Carbon (C) | ≤ 0.10 |
Manganese (Mn) | ≤ 0.5 |
Silicon (Si) | ≤ 0.5 |
Sulfur (S) | ≤ 0.01 |